Patent application number | Description | Published |
20110259848 | Rolled Copper Foil or Electrolytic Copper Foil for Electronic Circuit, and Method of Forming Electronic Circuit Using Same - Provided is a rolled copper foil or electrolytic copper foil for an electronic circuit to be used for forming a circuit by etching, wherein the rolled copper foil or the electrolytic copper foil comprises a nickel alloy layer with lower etching rate than copper, which is formed on an etching side of the copper foil, and the nickel alloy layer contains zinc. This invention aims to prevent sagging caused by the etching, to form a uniform circuit having the intended circuit width, and to shorten the time of forming a circuit by etching as much as possible, when forming a circuit by etching a copper foil of the copper-clad laminate; and also aims to make the thickness of the nickel alloy layer as thin as possible, to inhibit oxidation when exposed to heat, to prevent tarnish (discoloration) known as “YAKE”, to improve the etching properties in pattern etching, and to prevent the occurrence of short circuits and defects in the circuit width. | 10-27-2011 |
20110284496 | Method of Forming Electronic Circuit - Provided is a method of forming an electronic circuit, wherein a nickel or nickel alloy layer is formed on an etching side of a rolled copper foil or an electrolytic copper foil, the rolled copper foil or the electrolytic copper foil is bonded to a resin substrate to obtain a copper-clad laminate, a resist pattern for forming a circuit is subsequently applied on the copper foil, any unwanted portion of the copper foil and the nickel or nickel alloy layer of the copper-clad laminate other than the portion to which the resist pattern was applied is removed using an etching solution of an aqueous ferric chloride, the resist is further removed, and soft etching is additionally performed in order to remove the remnant nickel or nickel alloy layer and thereby form a circuit in which the space between copper circuit lines is of a width that is double or more from the thickness of copper. This invention aims to form a circuit with a uniform circuit width, improve the etching properties in pattern etching, and prevent the occurrence of short circuits and defects in the circuit width. | 11-24-2011 |
20110293960 | Rolled Copper Foil or Electrolytic Copper Foil for Electronic Circuit, and Method of Forming Electronic Circuit using same - Provided is a rolled copper foil or electrolytic copper foil for an electronic circuit to be used for forming a circuit by etching, wherein the copper foil comprises a heat resistance layer composed of zinc or zinc alloy or its oxide formed on an etching side of the rolled copper foil or electrolytic copper foil, and a layer of nickel or nickel alloy, which is a metal or alloy with a lower etching rate than copper, formed on the heat resistance layer. This invention aims to prevent sagging caused by the etching, to form a uniform circuit having the intended circuit width, and to shorten the time of forming a circuit by etching as much as possible, when forming a circuit by etching a copper foil of the copper-clad laminate; and also aims to make the thickness of the nickel or nickel alloy layer as thin as possible, to inhibit oxidation when exposed to heat, to prevent tarnish (discoloration) known as “YAKE”, to improve the etching properties in pattern etching, and to prevent the occurrence of short circuits and defects in the circuit width. | 12-01-2011 |
20110297641 | Rolled Copper Foil or Electrolytic Copper Foil for Electronic Circuit, and Method of Forming Electronic Circuit using same - Provided is a rolled copper foil or electrolytic copper foil for an electronic circuit to be used for forming a circuit by etching, wherein the copper foil comprises a nickel or nickel alloy layer with a lower etching rate than copper formed on an etching side of the rolled copper foil or electrolytic copper foil, and a heat resistance layer composed of zinc or zinc alloy or its oxide formed on the nickel or nickel alloy layer. This invention aims to prevent sagging caused by the etching, to form a uniform circuit having the intended circuit width, and to shorten the time of forming a circuit by etching as much as possible, when forming a circuit by etching a copper foil of the copper-clad laminate; and also aims to make the thickness of the nickel or nickel alloy layer as thin as possible, to inhibit oxidation when exposed to heat, to prevent tarnish (discoloration) known as “YAKS”, to improve the etching properties in pattern etching, and to prevent the occurrence of short circuits and defects in the circuit width. | 12-08-2011 |
20110300401 | Rolled Copper Foil or Electrolytic Copper Foil for Electronic Circuit, and Method of Forming Electronic Circuit using same - A rolled copper foil or electrolytic copper foil for an electronic circuit to be used for forming a circuit by etching, characterized in comprising a layer of metal of one or more types among a platinum group, gold and silver with an etching rate that is lower than the copper formed on an etching surface side of the rolled copper foil or the electrolytic copper foil, or alternatively comprising a layer of an alloy having the above-described metal as its main component. This invention aims to achieve the following upon forming a circuit by etching a copper foil of a copper clad laminate; specifically, to prevent sagging caused by the etching; to form a uniform circuit of the intended circuit width; to shorten the time of forming a circuit by etching as much as possible; to improve the etching properties in pattern etching; and to prevent the occurrence of short circuits and defects in the circuit width. | 12-08-2011 |
20120318568 | ELECTRONIC CIRCUIT, METHOD FOR FORMING SAME, AND COPPER CLAD LAMINATE FOR FORMING ELECTRONIC CIRCUIT - Provided is an electronic circuit as a laminated body configured from a layer (A) which is made of a copper or copper alloy foil formed on one surface or both surfaces of a resin substrate, a copper or copper alloy plated layer (B) formed on a part or whole surface of the (A) layer, a plated layer (C) formed on a part or whole surface of the (B) layer and having a slower etching rate than that of copper relative to a copper etching solution, and a copper or copper alloy plated layer (D) formed on the layer (C) and which has a thickness of 0.05 μm or more and less than 1 μm, and which is made of a copper circuit formed by etching and removing a part of the laminated portion of the (A) layer, the (B) layer, the (C) layer and the (D) layer up to the resin substrate surface. It is thereby possible to form a circuit having a uniform circuit width, improve the etching properties in pattern etching, and prevent the occurrence of short-circuits and defects in the circuit width. | 12-20-2012 |
20130270218 | Rolled Copper Foil or Electrolytic Copper Foil for Electronic Circuit, and Method of Forming Electronic Circuit Using Same - A rolled copper foil or electrolytic copper foil for an electronic circuit to be used for forming a circuit by etching, characterized in comprising a layer of metal of one or more types among a platinum group, gold and silver with an etching rate that is lower than the copper formed on an etching surface side of the rolled copper foil or the electrolytic copper foil, or alternatively comprising a layer of an alloy having the above-described metal as its main component. The following can be achieved upon forming a circuit by etching a copper foil of a copper clad laminate: sagging caused by the etching is prevented; a uniform circuit of the intended circuit width is formed; the time required to form a circuit by etching is reduced; etching properties in pattern etching are improved; and the occurrence of short circuits and defects in the circuit width are prevented. | 10-17-2013 |
20140093743 | Liquid Crystal Polymer Copper-Clad Laminate and Copper Foil Used For Said Laminate - Provided is a copper-clad laminate obtainable by bonding a copper foil on which roughening treatment including copper-cobalt-nickel alloy plating is performed and a liquid crystal polymer to each other, wherein the copper-clad laminate is free from a roughening particle residue on a surface of the liquid crystal polymer resin after copper foil circuit etching. The copper-clad laminate obtainable by bonding a copper foil and a liquid crystal polymer to each other, wherein the copper foil includes a copper primary particle layer formed on a surface bonded to the liquid crystal polymer and a secondary particle layer formed on the primary particle layer and made from a ternary alloy including copper, cobalt, and nickel; the primary particle layer has an average particle size of 0.25 to 0.45 μm; and the secondary particle layer has an average particle size of 0.05 to 0.25 μm. | 04-03-2014 |