Patent application number | Description | Published |
20080257516 | PRESSURE VESSEL, COMPRESSOR AND PROCESS FOR CASTING CYLINDER BLOCK - A pressure vessel of the present invention is such that at least part thereof comprises a metallic composite material | 10-23-2008 |
20080261067 | Metallic Composite Material - A metallic composite material according to the present invention is a metallic composite material, which comprises: a composited portion having a sintered body | 10-23-2008 |
20090136377 | Process for producing aluminum composite material - The present invention is such that it is an assignment to be solved to provide a process for producing aluminum composite material in which an iron sintered body of much higher adhesion is cast-in inserted with aluminum. | 05-28-2009 |
20090305917 | Sliding Material and Sliding Member Using the Sliding Material - To provide a sliding material whose superficial sliding characteristics can be modified in compliance with the requirements of sliding component parts without ever changing the surface roughness of sliding material very much by means of shot blasting treatment, and to provide a sliding member using the sliding material. | 12-10-2009 |
20100116378 | HEAT-RESISTANT MAGNESIUM ALLOY - A heat-resistant magnesium alloy according to the present invention includes Mg, a major component; a first alloying element “M | 05-13-2010 |
20100119405 | MAGNESIUM ALLOY FOR CASTING AND MAGNESIUM-ALLOY CAST PRODUCT - A magnesium alloy for casting according to the present invention is characterized in that, when the entirety is taken as 100% by mass, it includes copper (Cu) in an amount of from 1% by mass or more to 5% by mass or less, calcium (Ca) in an amount of from 0.1% by mass or more to 5% by mass or less, silver (Ag) in an amount of from 0.1% by mass or more to 5% by mass or less, and the balance comprising magnesium (Mg) and inevitable impurities. | 05-13-2010 |
20100209285 | MAGNESIUM ALLOY FOR CASTING AND MAGNESIUM-ALLOY CAST PRODUCT - A magnesium alloy for casting according to the present invention is characterized in that, when the entirety is taken as 100% by mass, it includes copper (Cu) in an amount of from 1% by mass or more to 5% by mass or less, calcium (Ca) in an amount of from 0.1% by mass or more to 5% by mass or less, tin (Sn) in an amount of from 0.1 or more to 3 or less by mass ratio with respect to the Ca (Sn/Ca); and the balance comprising magnesium (Mg) and inevitable impurities. | 08-19-2010 |
20110244326 | ELECTRODE FOR SECONDARY BATTERY AND MANUFACTURING PROCESS FOR THE SAME - It is an assignment to be solved to provide an electrode for secondary battery, electrode in which the active material is suppressed from coming off or falling down from the electricity collector, and that has excellent cyclic performance. | 10-06-2011 |