Patent application number | Description | Published |
20130130915 | SUBSTRATE FOR SUPERCONDUCTING WIRE ROD, SUPERCONDUCTING WIRE ROD, AND METHOD FOR PRODUCING SUPERCONDUCTING WIRE ROD - The phase transition temperature, at which the crystal lattice of LMO that constitutes an oxide layer as an intermediate layer or as a part of an intermediate layer becomes cubic, is lowered. A substrate for a superconducting wire rod includes an oxide layer (LMO layer ( | 05-23-2013 |
20130130916 | SUPERCONDUCTING THIN FILM AND METHOD OF MANUFACTURING SUPERCONDUCTING THIN FILM - Adhesiveness between a metallic substrate and a metal oxide layer is made to increase. A superconducting thin film ( | 05-23-2013 |
20130137580 | SUBSTRATE FOR SUPERCONDUCTING THIN FILM, SUPERCONDUCTING THIN FILM, AND METHOD OF PRODUCING SUPERCONDUCTING THIN FILM - An effect of suppressing diffusion of metal elements from a substrate is high and orientation of a forcibly-oriented layer is improved. A base material ( | 05-30-2013 |
20130157866 | SUPERCONDUCTING WIRE MATERIAL AND METHOD FOR MANUFACTURING SUPERCONDUCTING WIRE MATERIAL - Impurities in an oxide superconducting layer or at a surface of the oxide superconducting layer at an intermediate layer side are reduced. A superconducting wire rod has a configuration that includes a metal substrate | 06-20-2013 |
20130190188 | METHOD OF MANUFACTURING BASE MATERIAL FOR SUPERCONDUCTING CONDUCTOR, METHOD OF MANUFACTURING SUPERCONDUCTING CONDUCTOR, BASE MATERIAL FOR SUPERCONDUCTING CONDUCTOR, AND SUPERCONDUCTING CONDUCTOR - A method for manufacturing a base material | 07-25-2013 |
20130316908 | SUPERCONDUCTING WIRE ROD AND METHOD FOR MANUFACTURING SUPERCONDUCTING WIRE ROD - Impurities are reduced in an oxide superconducting layer and in an interface between the oxide superconducting layer and an intermediate layer. A superconducting wire rod | 11-28-2013 |
20150024942 | SUPERCONDUCTING WIRE - A superconducting wire has: a substrate; a superconducting layer that is layered on one main surface side of the substrate; a stabilization layer that covers a surface of the superconducting layer and another main surface of the substrate; and an insulating layer that covers a surface of the stabilization layer, and that has an identification portion that identifies the substrate side and the superconducting layer side. | 01-22-2015 |
20150357724 | Terminal, A Wire Connecting Structure and A Method of Manufacturing the Terminal - A terminal includes a connector portion, a tubular crimp portion that crimps/joins with a wire, and a transition portion joining the two portions. The tubular crimp portion is composed of a metal member including a base material of copper or copper alloy with 0.20-1.40 mm thickness and a coating layer of tin, tin alloy, nickel, nickel alloy, silver or silver alloy with 0.2-3.0 μm thickness formed on the base material. The tubular crimp portion has a weld portion formed by butt-welding and having, in its cross-section perpendicular to a terminal longitudinal direction, a phase existing therein of tin, tin alloy, nickel, nickel alloy, silver or silver alloy greater than 0.01 μm | 12-10-2015 |