Patent application number | Description | Published |
20080304206 | Raw Oil Composition for Carbon Material for Electric Double Layer Capacitor Electrode - The present invention provides a raw oil composition for manufacturing a carbon material for electric double layer capacitor electrodes, characterized in that the raw oil composition comprises 25 wt % or more of a saturated component and 16 wt % or less of an asphaltene component among the saturated component, an aromatic component, a resin component, and the asphaltene component obtained by developing of the raw oil composition by thin-layer chromatography; the raw oil composition has an average molecular weight of 960 or less; and the raw oil composition has an aromatic-carbon-fraction (fa) of 0.22 to 0.72. Use of the raw oil composition provides a carbon material for electric double layer capacitor electrodes that can exhibit high capacitance with high reproducibility without manufacturing synthetic pitch. | 12-11-2008 |
20110253593 | RAW COKE FOR ELECTRICITY STORAGE CARBON MATERIAL AND NEEDLE COKE - The present invention provides a raw coke having such a structure that the graphitized product resulting from graphitization of the raw coke at a temperature of 2800° C. under an inactive gas atmosphere will have ratios of the crystallite size to the lattice constant of 360 or less in the (002) plane and 1500 or less in the (110) plane, as a raw coke providing active carbon produced by alkali-activating the raw coke, which is reduced in remaining alkali content and can simplify washing operation because washing liquid can easily pass through the activated carbon, or as a raw coke for the production of needle coke. | 10-20-2011 |
20110267737 | RAW COKE FOR ELECTRICITY STORAGE CARBON MATERIAL AND NEEDLE COKE - The present invention provides a raw coke having such a structure that the graphitized product resulting from graphitization of the raw coke at a temperature of 2800° C. under an inactive gas atmosphere will have ratios of the crystallite size to the lattice constant of 360 or less in the ( | 11-03-2011 |
20120121987 | AMORPHOUS CARBON MATERIAL FOR NEGATIVE ELECTRODE OF LITHIUM ION SECONDARY BATTERY AND METHOD FOR PRODUCING THE SAME - The amorphous carbon material for the negative electrode of a lithium ion secondary battery of the invention has a true density of 1.800-2.165 g/cm | 05-17-2012 |
20120171572 | CARBON MATERIAL FOR NEGATIVE ELECTRODE OF LITHIUM SECONDARY BATTERY AND METHOD FOR PRODUCING THE SAME - To provide a negative electrode carbon material capable of suppressing capacity degradation which will occur due to repetition of a charge/discharge cycle, storage under a charged state, float charging, or the like. An artificial graphite for a negative electrode of a lithium secondary battery having a c-axis crystallite size L (112) of from 2.0 to 4.2 nm as calculated from a (112) diffraction line obtained by X-ray wide-angle diffractometry and having a half-value width Δν | 07-05-2012 |
20130089491 | RAW PETROLEUM COKE COMPOSITION FOR ANODE MATERIAL FOR LITHIUM ION SECONDARY BATTERY - Provided is a raw petroleum coke composition as a raw material of an anode carbon material that can improve, when a battery is discharged at a high current, the ratio capable of maintaining the capacity obtained during discharge at a low current. More specifically, provided is a raw petroleum coke composition for an anode carbon material of a lithium ion secondary battery, the raw petroleum coke composition being produced by subjecting a heavy-oil composition to a delayed coking process, and comprising an atomic ratio of hydrogen atoms H to carbon atoms C(H/C atomic ratio) of 0.30 to 0.50, and a micro-strength of 7 to 17% by weight. Further provided are a method for producing an anode carbon material of a lithium ion secondary battery, comprising the steps of: pulverizing the raw petroleum coke composition into particles having an average particle diameter of 5 to 30 μm, and subjecting the particles to carbonization and/or graphitization; and a lithium ion secondary battery comprising an anode comprising such a carbon material. | 04-11-2013 |
20130224101 | RAW MATERIAL CARBON COMPOSITION FOR NEGATIVE ELECTRODE MATERIAL OF LITHIUM-ION SECONDARY BATTERY - Provided is a raw material carbon composition for a negative electrode material for a lithium-ion secondary battery useful for achieving excellent high-speed charge and discharge characteristics. The raw material carbon composition is obtained by subjecting a stock oil composition to coking treatment, the stock oil composition being obtained by blending a stock oil (1) having a density at 15° C. of from 0.96 to 1.05 g/cm | 08-29-2013 |
20140079622 | CARBON MATERIAL FOR NEGATIVE ELECTRODE OF LITHIUM SECONDARY BATTERY AND METHOD FOR PRODUCING THE SAME - To provide a negative electrode carbon material capable of suppressing capacity degradation which will occur due to repetition of a charge/discharge cycle, storage under a charged state, float charging, or the like. An artificial graphite for a negative electrode of a lithium secondary battery having a c-axis crystallite size L (112) of from 2.0 to 4.2 nm as calculated from a (112) diffraction line obtained by X-ray wide-angle diffractometry and having a half-value width Δν | 03-20-2014 |