Skelhorn
David Skelhorn, Cumming, GA US
Patent application number | Description | Published |
---|---|---|
20130000518 | PAINT COMPRISING HYDROPHOBIZED MINERALS AND RELATED METHODS - A water-based paint composition may include at least one mineral treated with at least one hydrophobizing agent. The at least one mineral may include at least one of clay, kaolin, mica, titanium dioxide, talc, natural or synthetic silica or silicates, feldspars, nepheline syenite, talc, wollastonite, diatomite, barite, glass, and calcium carbonate. The at least one hydrophobizing agent may include at least one of fatty acids, fatty amines, and silanes. A method of making water-based paint may include treating at least one mineral with a hydrophobizing agent, and combining the at least one treated mineral with a binder. | 01-03-2013 |
David A. Skelhorn, Cumming, GA US
Patent application number | Description | Published |
---|---|---|
20100184348 | Spunlaid Fibers Comprising Coated Calcium Carbonate, Processes For Their Production, and Nonwoven Products - Disclosed herein, in one embodiment, are spunlaid fibers comprising at least one polymeric resin and at least one filler having an average particle size of less than or equal to about 5 microns and/or having a top cut of less than about 15 microns, wherein the at least one filler is present in an amount of less than about 40% by weight, relative to the total weight of the spunlaid fibers. Also disclosed herein is a method for producing spunlaid fibers comprising adding calcium carbonate to at least one polymeric resin and extruding the resulting mixture. Further disclosed herein are nonwoven fabrics comprising such spunlaid fibers and methods for producing them. | 07-22-2010 |
20120238175 | SPUNLAID FIBERS COMPRISING COATED CALCIUM CARBONATE, PROCESSES FOR THEIR PRODUCTION, AND NONWOVEN PRODUCTS - Disclosed herein are spunlaid fibers comprising at least one polymeric resin and at least one filler having an average particle size of less than or equal to about 5 microns and/or having a top cut of less than about 15 microns, wherein the at least one filler is present in an amount of less than about 40% by weight, relative to the total weight of the spunlaid fibers. Also disclosed herein is a method for producing spunlaid fibers comprising adding calcium carbonate to at least one polymeric resin and extruding the resulting mixture. Further disclosed herein are nonwoven fabrics comprising such spunlaid fibers and methods for producing them. | 09-20-2012 |
David A. Skelhorn, Alpharetta, GA US
Patent application number | Description | Published |
---|---|---|
20140070443 | Spunlaid Fibers Comprising Coated Calcium Carbonate, Processes for Their Production, and Nonwoven Products - Described herein are spunlaid fibers including at least one polymeric resin and at least one filler having an average particle size of less than or equal to about 5 microns and/or having a top cut of less than about 15 microns. The at least one filler may be present in an amount of less than about 40% by weight, relative to the total weight of the spunlaid fibers. Also described herein is a method for producing spunlaid fibers including adding calcium carbonate to at least one polymeric resin and extruding the resulting mixture. Further described herein are nonwoven fabrics including such spunlaid fibers, and methods for producing them. | 03-13-2014 |