Patent application number | Description | Published |
20090087766 | TONER FOR DEVELOPING ELECTROSTATIC LATENT IMAGE - The present invention relates to a toner for developing electrostatic latent images, comprising carbon black having a number average particle size of Feret's diameter of 5 to 300 nm and containing primary particles at a content of 5% or more on a number basis. | 04-02-2009 |
20100062362 | TONER FOR ELECTROPHOTOGRAPHY - An embodiment may be an electrophotographic toner which comprises at least one toner particle which comprises an inner layer and an outer layer covering the inner layer, wherein a cross-sectional area ratio of the outer layer to the inner layer is 0.05-0.46, and wherein a non-uniform thickness exists in the outer layer, and further the average thickness (t) taken at 5 positions as calculated by, is about 0.2-about 1.0 μm, t=(t | 03-11-2010 |
20100331488 | TUBULAR FLOW REACTOR AND METHOD FOR PRODUCING RESIN PARTICLE USING THE SAME - Provided is a tubular flow reactor containing: a cylindrical channel; a mixing shaft which is concentric with the cylindrical channel; and a mixing blade attached to the mixing shaft, wherein the tubular flow reactor satisfy the following requirements: t<2C and t/2C | 12-30-2010 |
20120095129 | RESIN COMPOSITION - Disclosed is a resin composition comprising (A) a polyester resin or a polycarbonate resin, (B) a polyethylene resin, (C) an aromatic compound other than the polyester resin and the polycarbonate resin, the aromatic compound having a residual carbon rate of not less than 20% by mass, and (D) a flame retardant, wherein the polyethylene resin is dispersed as crystal particles in the resin composition, and the content of the polyethylene resin crystal particles having a major axis diameter of 0.1 to 10 μm and an aspect ratio of 1 to 10 is not less than 60% by number based on the total polyethylene resin crystal particle number. The resin composition has high mechanical strength and excellent non-flammability | 04-19-2012 |
20120235327 | RECYCLED RESIN AND MANUFACTURING PROCESS THEREOF - Disclosed are a recycled resin manufacturing process and a recycled resin, the process comprising the steps of sorting a molded waste resin product, pulverizing the sorted molded waste resin product into resin flakes, washing the resin flakes, separating the washed resin flakes to remove different kinds of resins, drying the separated resin flakes, classifying the dried resin flakes to remove foreign matter deposited on the flakes, the classifying being carried out employing a classifying apparatus comprising a classifying section and provided therein, a physical field application device having an airflow force field and another physical field other than the airflow force field, and pelletizing the classified resin flakes, wherein the recycled resin has an oligomer content of not more than 1% by mass. | 09-20-2012 |
20130237644 | COPIER/PRINTER EXTERIOR PART USING HALOGEN-FREE FLAME-RETARDANT RESIN COMPOSITION INCLUDING RECYCLED POLYCARBONATE AND RECYCLED POLYETHYLENE TEREPHTHALATE - A copier/printer exterior part uses a halogen-free flame-retardant resin composition. The halogen-free flame-retardant resin composition includes 5 wt % to 50 wt % of unused polycarbonate, 20 wt % to 63 wt % of recycled polycarbonate, 5 wt % to 35 wt % of recycled polyethylene terephthalate, 0.2 wt % to 2 wt % of a styrene-acrylonitrile-glycidyl methacrylate terpolymer, 5 wt % to 15 wt % of a toughener, 10 wt % to 20 wt % of a flame retardant, 0.1 wt % to 0.8 wt % of a flame-retardant antidrip agent, 0.1 wt % to 1 wt % of an antioxidant, and 0.1 wt % to 2 wt % of a lubricant. The styrene-acrylonitrile-glycidyl methacrylate terpolymer includes 1 wt % to 5 wt % of glycidyl methacrylate and 20 wt % to 33 wt % of acrylonitrile. | 09-12-2013 |
20140296383 | COPIER/PRINTER EXTERIOR PART USING HALOGEN-FREE FLAME-RETARDANT RESIN COMPOSITION INCLUDING RECYCLED POLYCARBONATE AND RECYCLED POLYETHYLENE TEREPHTHALATE - A copier/printer exterior part uses a halogen-free flame-retardant resin composition. The halogen-free flame-retardant resin composition includes 5 wt % to 50 wt % of unused polycarbonate, 20 wt % to 63 wt % of recycled polycarbonate 5 wt % to 35 wt % of recycled polyethylene terephthalate, 0.2 wt % to 2 wt % of a styrene-acrylonitrile-glycidyl methacrylate terpolymer, 5 wt % to 15 wt % of a toughener, 10 wt % to 20 wt % of a flame retardant, 0.1 wt % to 0.8 wt % of a flame-retardant antidrip agent, 0.1 wt % to 1 wt % of an antioxidant, and 0.1 wt % to 2 wt % of a lubricant. The styrene-acrylonitrile-glycidyl methacrylate terpolymer includes 1 wt % to 5 wt % of glycidyl methacrylate and 20 wt % to 33 wt % of acrylonitrile. | 10-02-2014 |
20140371363 | THERMOPLASTIC RESIN COMPOSITION - A thermoplastic resin composition having a high flowability during the injection molding, which suppresses generation of burning, silver and the like in a molded article, is provided as an injection molding material. | 12-18-2014 |