Patent application number | Description | Published |
20090173668 | PROCESSING ASPHALTENE-CONTAINING TAILINGS - Embodiments of a method and a system for recovering energy, materials or both from asphaltene-containing tailings are disclosed. The asphaltene-containing tailings can be generated, for example, from a process for recovering hydrocarbons from oil sand. Embodiments of the method can include a flotation separation and a hydrophobic agglomeration separation. Flotation can be used to separate the asphaltene-containing tailings into an asphaltene-rich froth and an asphaltene-depleted aqueous phase. The asphaltene-rich froth, or an asphaltene-rich slurry formed from the asphaltene-rich froth, then can be separated into a heavy mineral concentrate and a light tailings. Hydrophobic agglomeration can be used to recover an asphaltene concentrate from the light tailings. Another flotation separation can be included to remove sulfur-containing minerals from the heavy mineral concentrate. Oxygen-containing minerals also can be recovered from the heavy mineral concentrate. Water removed by the various separation steps can be recycled and its heat energy recovered. | 07-09-2009 |
20090175769 | PROCESSING ASPHALTENE-CONTAINING TAILINGS - Embodiments of a method and a system for recovering energy, materials or both from asphaltene-containing tailings are disclosed. The asphaltene-containing tailings can be generated, for example, from a process for recovering hydrocarbons from oil sand. Embodiments of the method can include a flotation separation and a hydrophobic agglomeration separation. Flotation can be used to separate the asphaltene-containing tailings into an asphaltene-rich froth and an asphaltene-depleted aqueous phase. The asphaltene-rich froth, or an asphaltene-rich slurry formed from the asphaltene-rich froth, then can be separated into a heavy mineral concentrate and a light tailings. Hydrophobic agglomeration can be used to recover an asphaltene concentrate from the light tailings. Another flotation separation can be included to remove sulfur-containing minerals from the heavy mineral concentrate. Oxygen-containing minerals also can be recovered from the heavy mineral concentrate. Water removed by the various separation steps can be recycled and its heat energy recovered. | 07-09-2009 |
20090301937 | DRY,STACKABLE TAILINGS AND METHODS FOR PRODUCING THE SAME - Methods for preparing solvent-dry, stackable tailings. The methods may include a primary leaching or extraction process that separates most of the bitumen from a material comprising bitumen and produces first solvent-wet tailings. The first solvent-wet tailings are washed with a second solvent that removes the first solvent from the tailings. Second solvent remaining in the tailings is removed to thereby produce solvent-dry, stackable tailings. | 12-10-2009 |
20100032348 | METHODS FOR OBTAINING BITUMEN FROM BITUMINOUS MATERIALS - Methods for obtaining bitumen from bituminous material. The methods may include a dissolution step where a first solvent is added to material comprising bitumen to dissolve the bitumen contained therein. The majority of the dissolved bitumen is then removed from the mixture of first solvent and material comprising bitumen by filtering or settling the mixture of first solvent and material comprising bitumen. Any residual dissolved bitumen is then removed from the mixture of first solvent and material comprising bitumen by adding additional first solvent to the mixture to displace the residual dissolved bitumen from the mixture. | 02-11-2010 |
20110155648 | METHODS FOR OBTAINING BITUMEN FROM BITUMINOUS MATERIALS - A method of extracting bitumen from bituminous material. In some embodiments, the method may include loading a bitumen material in a column, followed by feeding a first quantity of first solvent into the column. The method may also include collecting the bitumen-enriched solvent exiting the column. A quantity of the bitumen-enriched solvent may then be fed into the column. In some embodiments, the method may include simultaneously loading bitumen material and a first solvent in a column, followed by feeding additional first solvent into the column. The method may also include collecting bitumen-enriched solvent exiting the column, and feeding a quantity of the bitumen-enriched solvent into the column. | 06-30-2011 |
20110180458 | METHODS FOR EXTRACTING BITUMEN FROM BITUMINOUS MATERIAL - Methods for preparing solvent-dry, stackable tailings. The method can include the steps of adding a first quantity of first solvent to a bitumen material to form a first mixture, separating a first quantity of bitumen-enriched solvent from the first mixture and thereby creating first solvent-wet tailings, adding a quantity of second solvent to first solvent-wet tailings to separate a first quantity of first solvent component from the first solvent-wet tailings and thereby producing second solvent-wet tailings, and adding a quantity of water to the second solvent-wet tailings to separate a first quantity of second solvent component from the second solvent-wet tailings and thereby forming solvent-dry, stackable tailings. | 07-28-2011 |
20110180459 | METHODS FOR EXTRACTING BITUMEN FROM BITUMINOUS MATERIAL - Methods for preparing solvent-dry, stackable tailings. The method can include the steps of adding a first quantity of first solvent to a bitumen material to form a first mixture, separating a first quantity of bitumen-enriched solvent from the first mixture and thereby creating first solvent-wet tailings, adding a quantity of second solvent to first solvent-wet tailings to separate a first quantity of first solvent component from the first solvent-wet tailings and thereby producing second solvent-wet tailings, and adding a quantity of water to the second solvent-wet tailings to separate a first quantity of second solvent component from the second solvent-wet tailings and thereby forming solvent-dry, stackable tailings. | 07-28-2011 |
20120145602 | PROCESS FOR EXTRACTING BITUMEN AND DRYING THE TAILINGS - A process for separating bitumen from bitumen ore material includes extracting bitumen with a hydrocarbon solvent to produce a bitumen-enriched solvent phase and tailings. The tailings are dried or stripped in a dryer to remove any remaining hydrocarbon solvent. The amount of solvent discharged in the tailings may be less than 4 bbl per 1000 bbl of recovered bitumen. | 06-14-2012 |
20120145603 | Process for Extracting Bitumen and Drying the Tailings - A process for separating bitumen from bitumen ore material includes extracting bitumen with a hydrocarbon solvent to produce a bitumen-enriched solvent phase and tailings. The tailings are dried or stripped in a dryer to remove any remaining hydrocarbon solvent. The amount of solvent discharged in the tailings may be less than 4 bbl per 1000 bbl of recovered bitumen. | 06-14-2012 |
20120151834 | Methods of Upgrading Asphaltene Compositions - Methods for pyrolyzing asphaltene material includes providing a composition including from 50 to 90 wt % asphaltene material and from 50 to 10 wt % inert material, and pyrolyzing the composition. The presence of the inert material can help to ensure that the asphaltene material does not interfere with the pyrolyzing process and equipment. Method of forming asphaltene pellets can also be used in order to improve asphaltene pyrolysis. | 06-21-2012 |
20120152809 | Methods and Apparatus for Bitumen Extraction - Methods and system for extracting bitumen can include the use of a mixing drum for spraying solvent over bituminous material to help dissolve bitumen and create a bitumen-laden solvent phase that can be separated from the non-bituminous components of the bituminous material. The mixing drum can be rotating during the spraying step to help promote dissolution of bitumen. The mixing drum can also include an internal screen for separating bitumen-laden solvent from the non-bituminous material. In some embodiments, two or more mixing drums are used in series, with the non-bituminous material from the first mixing drum being sprayed with additional solvent in the second mixing drum and bitumen laden solvent from the second mixing drum being used as the solvent sprayed over bituminous material in the first mixing drum. Hydrocyclones can also be incorporated in the in system and methods for increased extraction efficiency. | 06-21-2012 |
20120228196 | Methods of Preparing Bituminous Material for Bitumen Extraction - Methods of preparing bituminous material for extraction processing are described. The methods can include mixing bituminous material with hydrocarbon solvent before and/or during a step of crushing the bituminous material to reduce the size of clumps contained in the bituminous material. The steps of adding hydrocarbon solvent and crushing the bituminous material can be carried out multiple times. | 09-13-2012 |
20120305452 | Dry, Stackable Tailings and Methods for Producing the Same - Methods for preparing solvent-dry, stackable tailings. The methods may include a primary leaching or extraction process that separates most of the bitumen from a material comprising bitumen and produces first solvent-wet tailings. The first solvent-wet tailings are washed with a second solvent that removes the first solvent from the tailings. Second solvent remaining in the tailings is removed to thereby produce solvent-dry, stackable tailings. | 12-06-2012 |
20130006026 | Methods of Transporting Various Bitumen Extraction Products and Compositions Thereof - Methods for transporting bitumen extraction product include providing bitumen-laden aromatic solvent, providing bitumen-laden paraffinic solvent, and blending the two materials. The resulting mixture can be transported through existing pipeline infrastructure and can use existing separation processing equipment, and thereby avoids the need for separate infrastructure for each composition. Combining the two compositions can also avoid undesirable asphaltene precipitation. | 01-03-2013 |
20130025861 | Methods and Systems for In-Situ Extraction of Bitumen - A method for carrying out in-situ bitumen extraction can include a step of forming one or more vertical freeze walls within or around a deposit of bituminous material and establishing a laterally confined deposit of bituminous material; a step of injecting a solvent within the laterally confined deposit of bituminous material; a step of withdrawing a mixture of dissolved bitumen and solvent from within the laterally confined deposit of bituminous material; a step of injecting water within the laterally confined deposit of bituminous material; and a step of withdrawing a mixture of solvent and water from within the laterally confined deposit of bituminous material. | 01-31-2013 |
20130026076 | Methods for Obtaining Bitumen from Bituminous Materials - A method of extracting bitumen from bituminous material. In some embodiments, the method may include loading a bitumen material in a column, followed by feeding a first quantity of solvent into the column. The method may also include collecting the bitumen-enriched solvent exiting the column. A quantity of the bitumen-enriched solvent may then be fed into the column. In some embodiments, the method may include simultaneously loading bitumen material and a solvent in a column, followed by feeding additional solvent into the column. The method may also include collecting bitumen-enriched solvent exiting the column, and feeding a quantity of the bitumen-enriched solvent into the column. | 01-31-2013 |
20130026077 | Methods and Apparatus for Bitumen Extraction - A bitumen extraction method can include the use of a two or more mixing drums aligned in series for spraying solvent over bituminous material and/or tailings loaded in the mixing drums while the mixing drums rotate. Such mixing can result in the dissolution of bitumen into the solvent, which then allows for the separation of a “dilbit” stream from the bituminous material. | 01-31-2013 |
20130026078 | Methods for Extracting Bitumen From Bituminous Material - Methods for preparing solvent-dry, stackable tailings. The method can include the steps of adding a first quantity of solvent to a bitumen material to form a first mixture, separating a first quantity of bitumen-enriched solvent from the first mixture and thereby creating solvent-wet tailings, and adding a quantity of water to the solvent-wet tailings to separate a solvent component from the solvent-wet tailings and thereby forming solvent-dry, stackable tailings. The solvent used in the methods can include paraffinic solvent, such as pentane. | 01-31-2013 |
20130206405 | METHODS AND SYSTEMS FOR IN-SITU EXTRACTION OF BITUMEN - Methods and systems for in situ extraction of bitumen from deposits of bitumen-containing material are described. The methods and systems can generally include establishing freeze walls within the deposit of bitumen-containing material to establish a confined zone into which solvents can be injected in order to extract bitumen from the bitumen-containing deposits. Different types of solvents can be sequentially injected in order to extract bitumen and also help reduce the amount of solvent left behind in the deposit. | 08-15-2013 |
20130206647 | PROCESS FOR EXTRACTING BITUMEN AND DRYING THE TAILINGS - A process for separating bitumen from bitumen ore material includes extracting bitumen with a hydrocarbon solvent to produce a bitumen-enriched solvent phase and tailings. The tailings are dried or stripped in a dryer to remove any remaining hydrocarbon solvent. The amount of solvent discharged in the tailings may be less than 4 bbl per 1000 bbl of recovered bitumen. | 08-15-2013 |