Fombelle
Damien Fombelle, Chappes FR
Patent application number | Description | Published |
---|---|---|
20120115984 | Method for Making a Self-Sealing Composition - A process for manufacturing a self-sealing elastomer composition, said process comprising the following steps: a masterbatch, comprising at least one diene elastomer and more than 30 phr of a hydrocarbon resin, is firstly manufactured by compounding these various components in a mixer at a temperature or up to a temperature called the “hot compounding” temperature which is above the softening point of the hydrocarbon resin; and then at least one crosslinking system is incorporated into the masterbatch thus prepared, by compounding everything in the same mixer or in a different mixer, at a temperature or up to a temperature which is kept below 100° C., in order to obtain said self-sealing composition. | 05-10-2012 |
Damien Fombelle, Vebret FR
Patent application number | Description | Published |
---|---|---|
20120199260 | TIRE HAVING A BUILT-IN SELF-SEALING LAYER - A pneumatic tyre with a built-in self-sealing layer includes an outer rubbery tread, a carcass reinforcement, a gastight layer located at an inside position relative to the carcass reinforcement, a separable protective layer positioned innermost, and a self-sealing layer adjacent to the separable protective layer and located at an inside position relative to the gastight layer. The separable protective layer is a thermoplastic film that includes at least one fluoropolymer. | 08-09-2012 |
Damien Fombelle, Clermont-Ferrand FR
Patent application number | Description | Published |
---|---|---|
20140020806 | PNEUMATIC TIRE - A pneumatic tire provided with a noise damper in the tire cavity, which can maintain high-speed durability and productivity while also reducing cavity resonance, comprising a tread having a width TW in contact with the ground during travel, in which a noise damper made of a sound-absorbing material is attached to the tire internal surface in order to reduce cavity resonance, wherein the noise damper is at least one continuous ribbon made of a sound-absorbing material and having a width W and a thickness E, which is fixed over an attachment width Wc to the tire internal surface over a range of at least 30% of the inside of the tread in the radial direction, the start end and terminal end which are the two ends of the continuous ribbon are disposed in such a way as to be offset from each other in the axial direction, and the continuous ribbon forms, together with the tire internal surface, a continuous groove having a groove width D which is at least equal to 10% of the width W of the continuous ribbon. | 01-23-2014 |
20140048190 | PNEUMATIC TIRE - Provided is a pneumatic tire capable of yielding excellent water-draining performance, while reducing air column resonance. This pneumatic tire ( | 02-20-2014 |
Damlen Fombelle, Chappes FR
Patent application number | Description | Published |
---|---|---|
20110213050 | Process for Manufacturing a Self-Sealing Composition - Process for manufacturing a self-sealing elastomer composition, wherein the process comprises the following steps: firstly a masterbatch comprising at least one diene elastomer and a thermoplastic plasticizing hydrocarbon resin with a content greater than 30 phr is manufactured by compounding these various components in a mixer at a temperature or up to a temperature called the “hot compounding temperature” which is above the softening point of the hydrocarbon resin; and then at least one crosslinking system is incorporated into the masterbatch thus prepared, by compounding everything, in the same mixer or in a different mixer, at a temperature or up to a maximum temperature which is kept below 100° C., in order to obtain said self-sealing composition, and wherein at least one liquid plasticizer having a glass transition temperature (T | 09-01-2011 |
Damlen Fombelle, Clermont-Ferrand FR
Patent application number | Description | Published |
---|---|---|
20140014248 | PNEUMATIC TIRE AND METHOD FOR PRODUCING SAME - A method for producing a pneumatic tire in which a noise damper in the form of at least one continuous ribbon for reducing cavity resonance in a tire cavity is provided on the internal surface of a tire on the inside in the radial direction of the tire corresponding to the tire tread, including, providing a vulcanized and shaped tire; mixing a composition for forming the noise damper with a foaming agent to produce a liquid composition; rotating the tire in an upright state by means of a tire holding and rotation device, and introducing the liquid composition onto the tire internal surface by a device for introducing the liquid composition; varying the relative positional relationship of the pneumatic tire and the introduction implement in the axial direction of the tire while introducing the liquid composition is introduced onto the tire internal surface, and forming the liquid composition into a gel; and foaming and drying the gelled liquid composition. | 01-16-2014 |