Bucciotti
Francesco Bucciotti, Solignano (parma) IT
Patent application number | Description | Published |
---|---|---|
20120213911 | METHOD FOR THE REALIZATION OF BIOLOGICALLY COMPATIBLE PROSTHESIS - Method for the realization of a biologically compatible prosthesis component including the steps of having at least two materials with different physical/chemical features, defining in forming means the component as a composition of at least two volumes of at least two materials, sintering the component in the forming means and at a preset sintering temperature (T | 08-23-2012 |
Francesco Bucciotti, Civezzano IT
Patent application number | Description | Published |
---|---|---|
20140072641 | METHOD FOR THE REALISATION OF A BIOMATERIAL COMPRISING CALCIUM PHOSPHATE SHAPED AS GRANULES AND/OR THEIR AGGLOMERATES AND BIOMATERIAL OBTAINED WITH THIS METHOD - Method for the realization of a calcium phosphate-based biomaterial in form of granules and/or agglomerates of re-absorbable granules which can be used in the biomedical industry as, e.g., bone fillers, for increasing the bone mass, as a sealing for the internal orthopaedic prosthesis, for releasing drugs and/or medicaments and/or other substances beneficial for the organism. A calcium phosphate-based biomaterial in form of granules and/or aggregates thereof obtained according to such method. | 03-13-2014 |
Francesco Bucciotti, Civezzano (tn) IT
Patent application number | Description | Published |
---|---|---|
20150050326 | METHOD FOR THE REALIZATION OF A BIOCOMPATIBLE BONE IMPLANT COMPRISING GRANULAR ELEMENTS AND A BIOREABSORBABLE BIOPOLYMER GEL AND BIOCOMPATIBLE BONE IMPLANT THUS OBTAINED - Method for providing a biocompatible bone implant adapted to fill a bone cavity or lacuna including the steps of providing granular elements in form of granules and/or granule aggregates, providing at least one primary polymeric solution including a biopolymer, at least partly coating the granular elements with the primary polymeric solution, obtaining coated granular elements including a biopolymer coating, providing a cross-linking solution, dipping the coated granular elements in the cross-linking solution, waiting a period of time referred to as “jellification time” of between 30 seconds and 1 hour, in which during said waiting step there occurs the cross-linking of the biopolymer coating of the granular elements with the cross-linking solution and the jellification of the coating, with the aim of obtaining a cohesive biocompatible implant including granular elements and a bio-reabsorbable biopolymer gel; biocompatible bone implant obtained through such method. | 02-19-2015 |