Patent application number | Description | Published |
20130193480 | Epitaxy Technique for Reducing Threading Dislocations in Stressed Semiconductor Compounds - A solution for fabricating a semiconductor structure is provided. The semiconductor structure includes a plurality of semiconductor layers grown over a substrate using a set of epitaxial growth periods. During each epitaxial growth period, a first semiconductor layer having one of: a tensile stress or a compressive stress is grown followed by growth of a second semiconductor layer having the other of: the tensile stress or the compressive stress directly on the first semiconductor layer. One or more of a set of growth conditions, a thickness of one or both of the layers, and/or a lattice mismatch between the layers can be configured to create a target level of compressive and/or shear stress within a minimum percentage of the interface between the layers. | 08-01-2013 |
20130270519 | Non-Uniform Multiple Quantum Well Structure - A light emitting heterostructure including one or more fine structure regions is provided. The light emitting heterostructure can include a plurality of barriers alternating with a plurality of quantum wells. One or more of the barriers and/or quantum wells includes a fine structure region. The fine structure region includes a plurality of subscale features arranged in at least one of: a growth or a lateral direction. | 10-17-2013 |
20140110754 | Epitaxy Technique for Growing Semiconductor Compounds - A solution for fabricating a semiconductor structure is provided. The semiconductor structure includes a plurality of semiconductor layers grown over a substrate using a set of epitaxial growth periods. During each epitaxial growth period, a first semiconductor layer having one of: a tensile stress or a compressive stress is grown followed by growth of a second semiconductor layer having the other of: the tensile stress or the compressive stress directly on the first semiconductor layer. | 04-24-2014 |
20140134773 | Patterned Layer Design for Group III Nitride Layer Growth - A method of fabricating a device using a layer with a patterned surface for improving the growth of semiconductor layers, such as group III nitride-based semiconductor layers with a high concentration of aluminum, is provided. The patterned surface can include a substantially flat top surface and a plurality of stress reducing regions, such as openings. The substantially flat top surface can have a root mean square roughness less than approximately 0.5 nanometers, and the stress reducing regions can have a characteristic size between approximately 0.1 microns and approximately five microns and a depth of at least 0.2 microns. A layer of group-III nitride material can be grown on the first layer and have a thickness at least twice the characteristic size of the stress reducing regions. | 05-15-2014 |
20140326950 | Stress Relieving Semiconductor Layer - A semiconductor structure, such as a group III nitride-based semiconductor structure is provided. The semiconductor structure includes a cavity containing semiconductor layer. The cavity containing semiconductor layer can have a thickness greater than two monolayers and a multiple cavities. The cavities can have a characteristic size of at least one nanometer and a characteristic separation of at least five nanometers. | 11-06-2014 |
20150295133 | Semiconductor Heterostructure with Stress Management - A heterostructure for use in fabricating an optoelectronic device is provided. The heterostructure includes a layer, such as an n-type contact or cladding layer, that includes thin sub-layers inserted therein. The thin sub-layers can be spaced throughout the layer and separated by intervening sub-layers fabricated of the material for the layer. The thin sub-layers can have a distinct composition from the intervening sub-layers, which alters stresses present during growth of the heterostructure. | 10-15-2015 |
20150372193 | Patterned Layer Design for Group III Nitride Layer Growth - A device having a layer with a patterned surface for improving the growth of semiconductor layers, such as group III nitride-based semiconductor layers with a high concentration of aluminum, is provided. The patterned surface can include a substantially flat top surface and a plurality of stress reducing regions, such as openings. The substantially flat top surface can have a root mean square roughness less than approximately 0.5 nanometers, and the stress reducing regions can have a characteristic size between approximately 0.1 microns and approximately five microns and a depth of at least 0.2 microns. A layer of group-III nitride material can be grown on the first layer and have a thickness at least twice the characteristic size of the stress reducing regions. | 12-24-2015 |
20160035936 | Patterned Layer Design for Group III Nitride Layer Growth - A method of fabricating a device using a layer with a patterned surface for improving the growth of semiconductor layers, such as group III nitride-based semiconductor layers with a high concentration of aluminum, is provided. The patterned surface can include a substantially flat top surface and a plurality of stress reducing regions, such as openings. The substantially flat top surface can have a root mean square roughness less than approximately 0.5 nanometers, and the stress reducing regions can have a characteristic size between approximately 0.1 microns and approximately five microns and a depth of at least 0.2 microns. A layer of group-III nitride material can be grown on the first layer and have a thickness at least twice the characteristic size of the stress reducing regions. A device including one or more of these features also is provided. | 02-04-2016 |