Patent application number | Description | Published |
20120108729 | IMPACT-MODIFIED POLYCARBONATE/POLYESTER OR POLYCARBONATE/POLYAMIDE COMPOSITIONS - The invention relates to impact-modified polymer compositions, containing a polymer blend of polycarbonate with polyester and/or polyamide, plus an impact modifier blend of core/shell and functional polyolefin impact modifiers. The impact modifiers can provide the polymer blend composition with improved impact strength at equivalent loading, and also allow for higher amounts of polyester and/or polyamide in the blend without sacrificing impact strength. | 05-03-2012 |
20120157601 | PROCESS FOR CORE-SHELL IMPACT MODIFIERS AND IMPACT MODIFIED THERMOPLASTIC COMPOSITION WITH ENHANCED HYDROLYTIC RESISTANCE - The present invention relates to a process for producing impact modifiers, impact modified thermoplastic molding compositions and in particular impact modified polycarbonate or polycarbonate/polyester blends having improved resistance to degradation. More particularly the present invention relates to a process for producing polymeric impact modifiers with a core-shell structure made by a multistage process comprising a control and adjustment if necessary of the pH value before and during the recovery step. | 06-21-2012 |
20120157628 | IMPACT MODIFIED THERMOPLASTIC COMPOSITION WITH HYDROLYTIC SENSITIVITY TO OBTAIN HIGHER FLUIDITY WHILE KEEPING HIGH IMPACT STRENGTH - The present invention relates to, amongst other things, a process for manufacturing an impact modifier, concerns impact modified thermoplastic molding compositions and in particular a process for manufacturing and recovering the impact modifiers and their use in polymeric thermoplastic compositions. More particularly the present invention relates to a polymeric impact modifier with a core-shell structure manufactured by a multistage process comprising a special recovery process so that the composition of the thermoplastic polymer containing the impact modifier has a high fluidity while keeping its high impact strength. | 06-21-2012 |
20120157629 | CORE SHELL PARTICLE MULTISTAGE POLYMER POWDER, ITS MANUFACTURING PROCESS - The present invention relates to new impact modifiers and a process for making these new impact modifiers and their use in polymeric compositions. More particularly the present invention relates to a new polymeric impact modifier with a core-shell structure made by a multistage polymerization process comprising at least one gradient polymer. The present invention relates as well to a process preparing such an impact modifier, especially its recovery process after the end of the polymerization. The present invention also relates to a thermoplastic composition comprising the new impact modifier. | 06-21-2012 |
20120157630 | IMPACT MODIFIED THERMOPLASTIC COMPOSITION - The present invention relates to thermoplastic compositions comprising as impact modifier a rubber containing graft polymer prepared by the process of emulsion polymerization and recovered by a special process controlling and adjusting the value, the use of the thermoplastic compositions in the production of molded bodies, and to the molded, bodies themselves. The present invention relates also to thermoplastic compositions comprising a polymeric impact modifier with a core-shell structure made by a multistage process and recovered by a special process controlling and adjusting the pH value comprising at least one gradient polymer the use of the thermoplastic compositions in the production of molded bodies, and to the molded, bodies themselves. | 06-21-2012 |
20120271004 | METHOD FOR MANUFACTURING A POLYESTER COMPOSITION HAVING IMPROVED IMPACT PROPERTIES - The invention relates to a method for manufacturing a thermoplastic composition including: a polyester resin (c); a mixture including a copolymer (a) of an α-olefin and of a monomer having an ethylenic unsaturation and an epoxy function, as well as a core-shell compound (b); characterized in that said method includes a first step of manufacture the mixture of (a) and (b) by extrusion at a temperature at which the copolymer (a) is in the molten state and at a maximum temperature of 60 to 180° C.; a second step of manufacturing the thermoplastic composition by extrusion or by mixing the polyester resin (c) with the mixture of (a) and (b) produced in the first step. | 10-25-2012 |
20120316293 | POLYHYDROALKANOATE COMPOSITION EXHIBITING IMPROVED IMPACT RESISTANCE - A composition including polyhydroxyalkanoic acid (PHA), an elastomeric compound of core-shell type, and an olefinic copolymer including an ethylenic monomer bearing an epoxy function. The PHA composition exhibits improved impact strength. | 12-13-2012 |
20130281629 | NEW IMPACT MODIFIER AND IMPACT MODIFIED THERMOPLASTIC COMPOSITION - The invention relates to an impact modified thermoplastic resin comprising a polymeric impact modifier with a core-shell structure comprising 2-octylacrylate. | 10-24-2013 |
20140256848 | IMPACT-MODIFIED POLYCARBONATE/POLYESTER OR POLYCARBONATE/POLYAMIDE COMPOSITIONS - The invention relates to impact-modified polymer compositions, containing a polymer blend of polycarbonate with polyester and/or polyamide, plus an impact modifier blend of core/shell and functional polyolefin impact modifiers. The impact modifiers can provide the polymer blend composition with improved impact strength at equivalent loading, and also allow for higher amounts of polyester and/or polyamide in the blend without sacrificing impact strength. | 09-11-2014 |