Patent application number | Description | Published |
20130171456 | Glass Articles With Low-Friction Coatings - Low-friction coatings and glass articles with low-friction coatings are disclosed. According to one embodiment, a coated glass article may include a glass body comprising a first surface and a low-friction coating positioned on at least a portion of the first surface of the glass body. The low-friction coating may include a polymer chemical composition. The coated glass article may be thermally stable at a temperature of at least about 260° C. for 30 minutes. A light transmission through the coated glass article may be greater than or equal to about 55% of a light transmission through an uncoated glass article for wavelengths from about 400 nm to about 700 nm. The low-friction coating may have a mass loss of less than about 5% of its mass when heated from a temperature of 150° C. to 350° C. at a ramp rate of about 10° C./minute. | 07-04-2013 |
20130224407 | Glass Articles With Low-Friction Coatings - Low-friction coatings and glass articles with low-friction coatings are disclosed. According to one embodiment, a coated glass article may include a glass body comprising a first surface and a low-friction coating positioned on at least a portion of the first surface of the glass body. The low-friction coating may include a polymer chemical composition. The coated glass article may be thermally stable at a temperature of at least about 260° C. for 30 minutes. A light transmission through the coated glass article may be greater than or equal to about 55% of a light transmission through an uncoated glass article for wavelengths from about 400 nm to about 700 nm. The low-friction coating may have a mass loss of less than about 5% of its mass when heated from a temperature of 150° C. to 350° C. at a ramp rate of about 10° C./minute. | 08-29-2013 |
20140001076 | DELAMINATION RESISTANT GLASS CONTAINERS WITH HEAT-TOLERANT COATINGS | 01-02-2014 |
20140069886 | DELAMINATION RESISTANT GLASS CONTAINERS WITH HEAT-TOLERANT COATINGS - Delamination resistant glass containers with heat-tolerant coatings are disclosed. In one embodiment, a glass container may include a glass body having an interior surface, an exterior surface and a wall thickness extending from the exterior surface to the interior surface. At least the interior surface of the glass body is delamination resistant. The glass container may further include a heat-tolerant coating positioned on at least a portion of the exterior surface of the glass body. The heat-tolerant coating may be thermally stable at temperatures greater than or equal to 260° C. for 30 minutes. | 03-13-2014 |
20150084217 | MICRO-FEATURE METHODS FOR OVER-MOLDING SUBSTRATE - A method of making a microplate, including: injection molding a resin to form a substrate ( | 03-26-2015 |
20150085365 | LOW BIREFRINGENT SENSOR SUBSTRATE AND METHODS THEREOF - A resonant waveguide article, including: a polymeric substrate having at least one integral grating region, wherein the article has a low birefringence property of for example, from about 5 to 270 nm/cm, as defined herein. Also disclosed is a microplate including the resonant waveguide article, and an integral well plate bonded to the sensor article, as defined herein. Also disclosed are methods of making a sensor article, and a method of making and using the microplate including the sensor article, as defined herein. | 03-26-2015 |
20150329416 | GLASS ARTICLES WITH LOW-FRICTION COATINGS - Coated pharmaceutical packages are disclosed. In embodiments, a coated pharmaceutical package includes a glass body comprising a first surface. A low-friction coating may be positioned on at least a portion of the first surface of the glass body. The low-friction coating may include a polymer chemical composition. A light transmission through the coated pharmaceutical package may be greater than or equal to about 55% of a light transmission through an uncoated pharmaceutical package for wavelengths from about 400 nm to about 700 nm. The low-friction coating may have a mass loss of less than about 5% of its mass when heated from a temperature of 150° C. to 350° C. at a ramp rate of about 10° C./minute. | 11-19-2015 |
20150360999 | GLASS ARTICLES WITH LOW-FRICTION COATINGS - Coated pharmaceutical packages are disclosed. In embodiments, a coated pharmaceutical package may include a glass body comprising a first surface. A low-friction coating may be positioned on at least a portion of the first surface of the glass body. The low-friction coating may include a polymer chemical composition. The coated pharmaceutical package may be thermally stable at a temperature of at least about 260° C. for 30 minutes. The low-friction coating may have a mass loss of less than about 5% of its mass when heated from a temperature of 150° C. to 350° C. at a ramp rate of about 10° C./minute. | 12-17-2015 |