Patent application number | Description | Published |
20090139269 | Fiber Cure with Extended Irradiators - A method for producing an optical fiber that includes a method for producing an optical fiber, said method comprising: (i) drawing a bare optical fiber from a preform along a first pathway at a rate of at least 10 m/sec; (ii) contacting said bare optical fiber with a region of fluid in a fluid bearing and redirecting said bare optical fiber along a second pathway as said bare optical fiber is drawn across said region of fluid cushion; (iii) coating the bare optical fiber; and (iv) irradiating said coated fiber in at least one irradiation zone to at least partially cure said coating, while subjecting the optical fiber to UV light. | 06-04-2009 |
20090139270 | Fiber air turn for low attenuation fiber - A method for forming an optical fiber includes drawing the optical fiber from a glass supply and treating the fiber by maintaining the optical fiber in a treatment zone wherein the fiber is cooled at a specified cooling rate. The optical fiber treatment reduces the tendency of the optical fiber to increase in attenuation due to Rayleigh scattering, and/or over time following formation of the optical fiber due to heat aging. Methods for producing optical fibers along nonlinear paths incorporating fluid bearings are also provided thereby allowing for increased vertical space for the fiber treatment zone. | 06-04-2009 |
20090158779 | Methods and Systems For Producing Optical Fibers - Methods for producing a coated optical fiber may include drawing an optical fiber from a draw furnace along a first pathway and redirecting the optical fiber along a second, different pathway which is non-parallel with the first pathway. The optical fiber may be coated as it travels along the second pathway. | 06-25-2009 |
20090297722 | Methods and Systems For Producing Thermoplastic Coated Optical Fibers - A method for producing a coated optical fiber may include drawing an optical fiber from a draw furnace along a first vertical pathway. The optical fiber may then be routed through at least one fluid bearing thereby redirecting the optical fiber along a second vertical pathway. Thereafter, a thermoplastic coating may be applied to the optical fiber with a thermoplastic coating system. The optical fiber may then be wound onto a fiber storage spool with a fiber take-up system. The fiber take-up system may be space apart from the thermoplastic coating system such that the thermoplastic coating may be cooled before the optical fiber is wound onto the fiber storage spool. | 12-03-2009 |
20100281922 | Methods for producing optical fibers - Methods for producing optical fibers along nonlinear paths include incorporating fluid bearings. An optical fiber is drawn from a preform along a first pathway, contacted with a region of fluid cushion of a fluid bearing, and redirected along a second pathway as the fiber is drawn across said region of fluid cushion. | 11-11-2010 |
20110094717 | Systems and Methods for Cooling Optical Fiber - In one embodiment, an optical fiber cooling system includes a first cooling tube oriented substantially in parallel with and spaced apart from a second cooling tube such that an optical fiber pathway is positioned between the first cooling tube and the second cooling tube. The first cooling tube includes a plurality of cooling fluid outlets positioned along an axial length of the first cooling tube which are oriented to direct a flow of cooling fluid across the optical fiber pathway towards the second cooling tube. The second cooling tube includes a plurality of cooling fluid outlets positioned along an axial length of the second cooling tube which are oriented to direct a flow of cooling fluid across the optical fiber pathway towards the first cooling tube. | 04-28-2011 |
20110289979 | METHOD FOR PRODUCTING OPTICAL FIBER AT REDUCED PRESSURE - An optical fiber production system and method are provided for producing optical fiber. An optical fiber is drawn from a preform in a furnace and passes through a treatment device under a reduced pressure in the range of 0.01 to 0.80 atm. The treatment device cools the bare optical fiber as it cools to a temperature in the range of at least 1,600° C. to 1,300° C. A non-contact fiber centering device is located near an exit of the treatment device to provide centering of the optical fiber as it exits the treatment device. | 12-01-2011 |
20110289980 | METHOD FOR PRODUCING OPTICAL FIBER USING LINEAR NON-CONTACT FIBER CENTERING - An optical fiber production system and method are provided for producing optical fiber. An optical fiber is drawn from a preform in a furnace and passes through a treatment device under a controlled reduced pressure or partial vacuum in the range of 0.01 to 0.8 atm. The treatment device cools the bare optical fiber as it cools to a temperature range of at least 1,600° C. to 1,300° C. A non-contact fiber centering device is located near an exit of the treatment device to provide linear centering of the optical fiber as it exits the treatment device. | 12-01-2011 |
20120260697 | SYSTEMS AND METHODS FOR COOLING OPTICAL FIBER - In one embodiment, an optical fiber cooling system includes a first cooling tube oriented substantially in parallel with and spaced apart from a second cooling tube such that an optical fiber pathway is positioned between the first cooling tube and the second cooling tube. The first cooling tube includes a plurality of cooling fluid outlets positioned along an axial length of the first cooling tube which are oriented to direct a flow of cooling fluid across the optical fiber pathway towards the second cooling tube. The second cooling tube includes a plurality of cooling fluid outlets positioned along an axial length of the second cooling tube which are oriented to direct a flow of cooling fluid across the optical fiber pathway towards the first cooling tube. | 10-18-2012 |
20130255397 | OPTICAL FIBER TENSILE SCREENING METHOD AND DEVICE - A method and device for continuously testing the tensile strength of an optical fiber, wherein the incoming optical fiber is wrapped at least partially around a payout capstan, to an intermediate payout pulley, at least partially around the intermediate payout pulley, and back to the payout capstan. The optical fiber is then wound from the payout capstan to a tensile testing measurement component, and then to an uptake capstan. The optical fiber is wrapped at least partially around the uptake capstan, to an intermediate uptake pulley, at least partially around the intermediate uptake pulley, and back to the uptake capstan. The payout capstan and uptake capstan are operated at a desired rotational speed to continuously advance the optical fiber for tensile strength testing. | 10-03-2013 |
20130312461 | METHOD FOR COOLING OPTICAL FIBER - In one embodiment, an optical fiber cooling system includes a first cooling tube oriented substantially in parallel with and spaced apart from a second cooling tube such that an optical fiber pathway is positioned between the first cooling tube and the second cooling tube. The first cooling tube includes a plurality of cooling fluid outlets positioned along an axial length of the first cooling tube which are oriented to direct a flow of cooling fluid across the optical fiber pathway towards the second cooling tube. The second cooling tube includes a plurality of cooling fluid outlets positioned along an axial length of the second cooling tube which are oriented to direct a flow of cooling fluid across the optical fiber pathway towards the first cooling tube. | 11-28-2013 |